Abstract
This invention concerns an improvement in cast iron material and chilled iron material. The cast iron material has a C.E. value of not more than 4.3 in which cerium is added in the form of a mischmetal upon casting to a cerium content of from 0.005 to 0.035 wt %. The chilled cast iron article has a chilled layer formed by remelting at least a portion of the surface of the cast iron of a predetermined shape composed of the above-mentioned cast iron by a high density energy source such as tungsten inert gas (TIG) arc, laser or electron beam.