Patent · US Expired

Process for making a dehydrogenation catalyst having improved moisture stability

US4684619A · kind A · utility

11Cited by
2References
5Claims
0Family size

Assignee

Inventor

Key dates

Filing dateSep 30, 1986
Grant dateAug 4, 1987
Priority date
Expiry dateSep 30, 2006

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC07C5/3332
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A method for preparing an iron oxide containing dehydrogenative catalyst having improved moisture stability which comprises calcining by a two step method. The temperature of calcination is maintained at from about 250.degree. to about 600.degree. C. in the first step and from about 700.degree. to about 800.degree. C. in the second step. The effectiveness of the catalyst is not substantially changed from that of the single step calcination known to the art while the moisture stability is improved.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.