Patent · US Expired

Method for the multi-stage fibre cables and the apparatus required for it

US4701980A · kind A · utility

0Cited by
10References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 3, 1986
Grant dateOct 27, 1987
Priority date
Expiry dateApr 3, 2006

Classification

  • Technology area (CPC D)Textiles; Paper
  • CPC primaryD02G1/20
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

An improved method for the after-treatment of washed and dried fibre cable having a minimum mass of 250 ktex by crimping, fixing, cooling and optionally cutting or tearing is achieved in that the band width of the cable issuing from the drier with a covering density of at most 5 ktex/cm is reduced by at least 50% of the original band width with a corresponding increase in the packing density, is crimped in a stuffer box crimping means at a stuffer box pressure of from 4 to 10 N/cm and a stuffer box temperature of from 80.degree. to 95.degree. C., the crimping is fixed in or immediately after the stuffer box, the cable is deposited on the surface of an air-permeable conveyor belt, air is blown or sucked there through fibre package or conveyor belt and the cable is then optionally supplied to a tearing converter or a cutting machine.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.