Abstract
Uranium is recovered as UF.sub.4 from phosphate solutions. The uranium is reduced to the tetravalent state and extracted with an organic extractant. The uranium is recovered as UF.sub.4 by reextracting with an aqueous HF solution which includes UF.sub.4 in suspension for improved reextraction.