Processing of copper alloys and product
US4724013A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Nov 5, 1985 |
| Grant date | Feb 9, 1988 |
| Priority date | — |
| Expiry date | Nov 5, 2005 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB23K35/222
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
This invention is directed to the treatment of copper beryllium alloys, and to articles and parts made therefrom, containing special small amounts of beryllium and cobalt, e.g., about 0.2% to about 0.5% beryllium and about 0.2% to about 1% or about 1.5% or about 2% cobalt, which imparts to these alloys a superior combination of stress relaxation resistance, formability, ductility, conductivity and strength by the process of solution annealing, cold working at least about 50% or at least about 70% or 90% or more and age hardening.