Patent · US Expired

Alumina ceramic body

US4735926A · kind A · utility

16Cited by
2References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 14, 1986
Grant dateApr 5, 1988
Priority date
Expiry dateMar 14, 2006

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B35/111
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A dielectric alumina ceramic body having a constant dielectric loss tangent tan .delta. is obtained by sintering a composition consisting essentially of: PA1 100 parts by weight of a ternary formulation consisting of 92.4 to 98.7 mol % Al.sub.2 O.sub.3, at least 0.5 mol % CaO, and 1.3 to 7.6 mol % TiO.sub.2 ; and PA1 at least one selected from the group consisting of Cr.sub.2 O.sub.3 and NiO subject to the relation of: ##EQU1## where x is the weight part of Cr.sub.2 O.sub.3 per 100 parts by weight of said formulation, PA1 y is the weight part of NiO per 100 parts by weight of said formulation, and PA1 z is the mol % of Al.sub.2 O.sub.3 in the formulation, PA1 provided that x.gtoreq.0 and y.gtoreq.0, except x=y=0.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.