Patent · US Expired

Elastomer with improved high temperature characteristics

US4753989A · kind A · utility

2Cited by
7References
5Claims
0Family size

Assignee

Inventor

Key dates

Filing dateMar 25, 1987
Grant dateJun 28, 1988
Priority date
Expiry dateMar 25, 2007

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10S525/905
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A soft thermoplastic, elastomeric alloy containing a thermoplastic, elastomeric block copolymer material, a polyethylene, and a polyphenylene ether material, prepared by blending in an extruder with an L/D ratio equal to or greater than 30 to 1. The alloy comprises a blend of from about 80 to 98% thermoplastic, elastomeric block copolymer material; from about 1 to 10% by weight of low melt index, highly crystalline polyethylene; and from about 1 to 10% by weight of polyphenylene ether. The material demonstrates excellent creep resistance at elevated temperatures as well as a variety of other excellent physical properties.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.