Improved process for beneficating iron-containing titaniferous ores

US4762552A · kind A · utility

5Cited by
4References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 15, 1987
Grant dateAug 9, 1988
Priority date
Expiry dateJun 15, 2007

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22B34/1245
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The beneficiation or upgrading of an iron-containing titaniferous ore to a synthetic rutile by subjecting the ore to reduction followed by acid leaching of the reduced ore is improved by forming a mixture of the ore and an aqueous sulfuric acid solution, adding a reducing agent to this mixture and then subjecting this mixture containing the reducing agent to reduction at elevated temperatures. The resulting reduced ore, which is characterized by an increase in the ferrous iron content thereof and an increase in its specific surface area, exhibits an enhanced response to subsequent acid leaching to provide a synthetic rutile of improved purity.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.