A mechanical disintegration is effected in which substantially only the metal sheath of the small batteries is torn apart. The crushed material is roasted at 500.degree. to 1000.degree. C. in a state of motion in an oxidizing atmosphere and the volatilized mercury is recovered from the exhaust gas. The roasted material is separated by sieving and magnetic separation into an iron-containing scrap fraction, a brass-containing scrap fraction and a collectable fraction, which contains manganese, zinc and silver.