Patent · US Expired

Drying low rank coal and retarding spontaneous ignition

US4775390A · kind A · utility

3Cited by
7References
13Claims
0Family size

Assignee

Inventor

Key dates

Filing dateDec 10, 1987
Grant dateOct 4, 1988
Priority date
Expiry dateDec 10, 2007

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC10L9/00
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

Coal is rendered less subject to abrasion and disintegration by reducing it to a 0.2 to 0.5-inch particle size and drying it in a drying zone at a temperature of 200.degree. to 230.degree. F. for 3-7 minutes while simultaneously applying a treating agent which can be a light cycle oil, heavy cycle oil, clarified slurry oil, a petroleum or coal derived distillate or residuum, a solution of durene in gasoline and mixtures of two or more of the preceding.