Method and apparatus for controlling weld bead shape to eliminate microfissure defects when shape melting austenitic materials
US4782206A · kind A · utility
28Cited by
5References
10Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jan 27, 1987 |
| Grant date | Nov 1, 1988 |
| Priority date | — |
| Expiry date | Jan 27, 2007 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB23K9/048
- WIPO fieldMachine tools
- WIPO sectorMechanical engineering
Abstract
A method and apparatus for eliminating microfissure defects in shape melted austenitic material components by closely controlling the deposited weld bead shape to a geometry where the underbead shape has no sharp discontinuties. Oscillation of the welding torch head during the process is used to smooth out the weldbead shape and is especially adapted for use with gas metal-arc welding processes.