Method for passivating low rank dried coal
US4783200A · kind A · utility
3Cited by
1References
9Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jun 8, 1987 |
| Grant date | Nov 8, 1988 |
| Priority date | — |
| Expiry date | Jun 8, 2007 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC10L9/10
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
Coal is rendered less subject to abrasion and disintegration by reducing it to a 0.2 to 0.5-inch particle size and drying it at a temperature of 200.degree. to 230.degree. F. for 3-7 minutes. The coal is rendered less susceptible to spontaneous ignition by the application of a treating agent which is a petroleum resid mixed with clarified slurry oil or a petroleum resid mixed with a distillate.