A high strength aluminum alloy including 5 to 13 wt % Si, 1 to 5 wt % Cu, 0.1 to 0.5 wt % Mg, 0.005 to 0.3 wt % Sr, and the balance Al and inevitable impurities. The aluminum alloy is subjected to pressure casting and T6 heat treatment. The solution treatment time can be shortened.