Patent · US Expired

Time effective method for preparing ferrierite

US4795623A · kind A · utility

22Cited by
13References
15Claims
0Family size

Assignee

Inventor

Key dates

Filing dateAug 5, 1986
Grant dateJan 3, 1989
Priority date
Expiry dateAug 5, 2006

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10S423/23
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

This invention concerns a time-effective method of manufacture for a sodium ferrierite precursor of a hydrogen ferrierite catalytic composition of matter by crystallizing an aqueous admixture of sodium hydroxide, an aluminum compound, a silicon compound and a nitrogen-containing compound, which mixture possesses 1.60 to 3.40 moles of sodium oxide and 0.70 to 1.60 moles of aluminum oxide per 25 moles of silicon oxide. The ultimate use of the resultant catalyst is for excising wax from a lubricating oil (preferably a light lubricating oil) with or without the presence of metals of Group VIII and Group VIB on the catalyst.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.