Abstract
Superalloy with oxide dispersion hardening having improved corrosion and oxidation resistance and based on nickel with the following composition: PA1 Cr=17-18% by weight, PA1 Al=6-7% by weight, PA1 Mo=2-2.5% by weight, PA1 W=3-3.5% by weight, PA1 Ta=2-2.5% by weight, PA1 Zr<0.2% by weight, PA1 B<0.02% by weight, PA1 C<0.1% by weight, PA1 Y.sub.2 O.sub.3 =1-1.5% by weight, PA1 Ni=Remainder.