Nickel-base alloy heat treatment
US4798633A · kind A · utility
9Cited by
2References
10Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Sep 25, 1986 |
| Grant date | Jan 17, 1989 |
| Priority date | — |
| Expiry date | Sep 25, 2006 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S376/90
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A process for heat treating certain nickel-chromium-iron alloys is disclosed which involves annealing the alloys over the temperature range of 1750.degree. F. to 2150.degree. F., preferably in a continuous annealing furnace, for short periods of time, such as 30 minutes to 2 hours, the time being sufficient to precipitate carbides at the alloy grain boundaries. The alloys are useful in nuclear reactor environments.