Room temperature crosslinkable compositions
US4801673A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jul 6, 1987 |
| Grant date | Jan 31, 1989 |
| Priority date | — |
| Expiry date | Jul 6, 2007 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S528/901
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Compositions which are storable under anhydrous conditions, but when exposed to atmospheric moisture crosslink at room temperature to form elastomers comprising a diorganopolysiloxane having one Si-bonded hydroxyl group in each of its terminal units, and a cyclic silane of the formula ##STR1## where R represents a divalent hydrocarbon radical, R.sup.1 represents the same or different monovalent hydrocarbon radicals, which can be substituted by an alkoxy group, and R.sup.2 represents hydrogen or an alkyl or aminoalkyl radical in which the silicon atom of the cyclic silane is bonded to a nitrogen atom and to two monovalent hydrocarbon radicals, which can be substituted with an alkoxy group via oxygen and to a hydrocarbon radical via carbon.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.