Single-crystal Ni-based super-heat-resistant alloy
US4802934A · kind A · utility
7Cited by
1References
6Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Nov 5, 1986 |
| Grant date | Feb 7, 1989 |
| Priority date | — |
| Expiry date | Nov 5, 2006 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C19/056
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A single-crystal Ni-based super-heat-resistant alloy consisting essentially of, by weight percentage, 4 to 10% of Cr, 4 to 6.5% of Al, 4 to 10% of W, 4 to 9% of Ta, 1.5 to 6% of Mo, and the balance substantially Ni and impurities; or the alloy containing not greater than 12% of Co in addition to the above composition; wherein the contents of W, Ta and Mo are selected to meet the following condition: 1/2.W+1/2.Ta+Mo=9.5% to 13.5%.