Butt-welded cans and process for manufacturing the same

US4805795A · kind A · utility

4Cited by
3References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 28, 1987
Grant dateFeb 21, 1989
Priority date
Expiry dateDec 28, 2007

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/1355
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

There is here provided butt-welded cans made of steel plates having a carbon concentration of 0.02 to 0.09% by weight, the aforesaid butt-welded cans being characterized in that a coating film for preventing the adhesion of melted metal particles is applied to at least the inner surface of the weld portion and its vicinity of each can, and a carbon concentration index I of the weld portion satisfies the formula (1) EQU I=(Iw/Ic).times.10.sup.3 .ltoreq.15 (1) wherein Iw is a K.alpha. X ray intensity, of carbon in the weld portion, measured by the EPMA method, and PA0 Ic is a K.alpha. X ray intensity, of carbon in graphite, measured by the EPMA method.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.