Abstract

An anodized aluminum product prepared by anodizing an alloy comprising 1.20-1.60% iron and 0.25-0.55% manganese with a weight ratio of iron to manganese between 2.8 and 5, up to 0.20% silicon, up to 0.30% copper, up to 5% magnesium, up to 0.10% chromium, up to 2% zinc, up to 0.25% zirconium, up to 0.10% titanium, remainder aluminum and in total up to 0.50% of other by anodic oxidation in an electrolyte at a temperature of less than 560.degree. C. for no more than 4 hours so as to produce an oxide thickness of 5 to 30 .mu.m.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.