Abstract
A new SAE 1541M alloy steel composition consisting essentially of 0.40-0.48% carbon, 1.35-1.61% maganese, 0.16-0.30% silicon, 0-0.23% chromium and the balance iron and other materials not affecting hardenability of the steel, especially adapted for forming axle shafts in the 1.70-2.05" diameter range to be used as drive axles with an axle load carrying capacity between 30,000 and 44,000 pounds.