Co-deposition of fluorinated carbon with electroless nickel
US4830889A · kind A · utility
33Cited by
4References
10Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Sep 21, 1987 |
| Grant date | May 16, 1989 |
| Priority date | — |
| Expiry date | Sep 21, 2007 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC23C18/34
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
A process for co-depositing fluorinated carbon with electroless nickel which provides a uniformly dispersed co-deposit. The process includes the use of a non-ionic, wetting agent in combination with a cationic wetting agent for the suspension of fluoronated carbon in the electroless nickel solution.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.