Abstract
Low viscosity polymer polyols having high styrene/acrylonitrile ratios and good stability may be achieved by the use of a base polyol having a molecular weight higher than 4000, for example, from 4000 to 6500 and a high molecular weight (HMW) dispersant. The dispersant polyol may range from 1 to 20 wt. %, but may be less than 5 wt. % of the total polyol component of the polymer polyol. The HMW dispersant should have a molecular weight higher than about 6000. Preferably, a semi-batch reactor is used, and a relatively high concentration of the HMW dispersant is initially charged to the reactor, relative to the portion of base polyol. Monomer ratios of styrene to acrylonitrile of 85/15 may be achieved with this method.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.