Process for the preparation of epoxidized polybutadienes
US4851556A · kind A · utility
4Cited by
7References
5Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 2, 1988 |
| Grant date | Jul 25, 1989 |
| Priority date | — |
| Expiry date | Mar 2, 2008 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08C19/06
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Epoxidized polybutadienes with an average molecular weight of 500 to 100,000 and a certain content of epoxide oxygen were prepared from the corresponding polybutadienes with use of perpropionic acid in a benzene solution. The solution can also be employed in unpurified form with maximum contents of 1.5 weight percent hydrogen peroxide 1.5 weight percent of water, and about 800 ppm of mineral acid.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.