High temperature low thermal expansion ceramic
US4855265A · kind A · utility
43Cited by
4References
12Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Apr 4, 1988 |
| Grant date | Aug 8, 1989 |
| Priority date | — |
| Expiry date | Apr 4, 2008 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC04B35/478
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
This invention relates to the high temperature stabilization of aluminum titanate and aluminum titanate-mullite compositions by the addition of iron oxide. It has been found that iron oxide concentrations greater than 5 weight percent and as high as approximately 25 weight percent have a stabilization effect at high temperatures on aluminum titanates. The resultant ceramic body is further enhanced by the addition of from 0.1 to 5 weight percent rare earth oxide.