Battery element and method for making same
US4861689A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Nov 23, 1987 |
| Grant date | Aug 29, 1989 |
| Priority date | — |
| Expiry date | Nov 23, 2007 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T29/49115
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
In a method for producing a battery element useful as at least a positive plate in a lead-acid battery, the element comprising a fluid impervious, electrically conductive matrix having mutually opposing first and second surfaces and positive active electrode material associated with the first surface of the matrix, the improvement which comprises: PA0 conditioning the first surface to enhance the association of the positive active electrode material and the first surface; and PA0 applying and associating the positive active electrode material to the first surface.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.