An iron/copper/chromium alloy material for a high-strength lead frame or pin grid array, which comprises 20 to 90% by weight of Cu and 2.5 to 12% by weight of Cr, with the balance being mainly iron, and which has an average grain size number of at least 10 in each of the iron/chromium phase and the copper phase, is prepared by continuous casting, cold-working, and aging.