Patent · US Expired

Method of producing a quick-curing novolac phenolic resin using ammonium halides

US4870154A · kind A · utility

5Cited by
3References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 20, 1987
Grant dateSep 26, 1989
Priority date
Expiry dateNov 20, 2007

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08G8/10
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A method of producing a novolac phenolic resin having quick-curing properties and good fluidity is disclosed, whereby the novolac resin is prepared by reacting a phenol with an aldehyde using an acidic catalyst and thereafter adding an ammonium halide. The ammonium halide is added in amounts of about 0.05 to 3 wt % of the solid resin, and the conversion of aldehyde is not less than 90% and the water content of the resin is not less than 5%.