Graphite structures and method for production thereof
US4873071A · kind A · utility
22Cited by
9References
4Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Apr 28, 1988 |
| Grant date | Oct 10, 1989 |
| Priority date | — |
| Expiry date | Apr 28, 2008 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2006/11
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A graphite structure, which is of light weight and excellent elasticity and has a packing density of 0.5 g/cm.sup.3 or lower and a recovery of 50% or higher at a compressibility of 10 to 90%, is obtained by treating a carbonaceous material with nitric acid or a mixture of nitric and sulfuric acids and, then, heat-treating the obtained product at a temperature of 2,400.degree. C. or higher to graphitize the same.