Stabilization of poly(arylene ether ketones)

US4874839A · kind A · utility

7Cited by
11References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 5, 1988
Grant dateOct 17, 1989
Priority date
Expiry dateAug 5, 2008

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08G65/46
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A method of stabilizing a poly(arylene ether ketone), which method comprises in one embodiment heating the poly(arylene ether ketone) at a temperature between about 240.degree. C. and about 325.degree. C. for a period of between about 0.5 and about 24 hours, prior to any melt-processing of the poly(arylene ether ketone) and in another embodiment hydrothermally treating the poly(arylene ether ketone) by heating it to a temperature of at least 160.degree. C. while contacting it with water.