Patent · US Expired

Sintered form body

US4895815A · kind A · utility

7Cited by
3References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 3, 1987
Grant dateJan 23, 1990
Priority date
Expiry dateDec 3, 2007

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B35/478
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Disclosed is a starting mixture for the preparation of a sintered body on a basis of aluminum titanate consists of more than 46 wt.-% TiO.sub.2, up to 49.5 wt.-% Al.sub.2 O.sub.3, 3 to 5 wt.-% quartz, and less than 0.2 wt.-% impurities, Al.sub.2 O.sub.3 and TiO.sub.2 being present in the weight ratio of 1:0.95 to 1:1.05. The sintered body according to the invention is composed of: PA1 15 to 35 wt.-% TiO.sub.2 ; PA1 60 to 85 wt.-% Al.sub.2 TiO.sub.5 (aluminum titanate); PA1 up to 5 wt.-% Al.sub.2 O.sub.3 ; PA1 up to 17 wt.-% Mullite; and PA1 max. 0.2 wt.-% impurities, all parts by weight together totaling 100 wt.-%. Also disclosed are processes for making the sintered body.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.