Patent · US Expired

Stretched poly(arylene thioether-ketone) films and production process thereof

US4895912A · kind A · utility

8Cited by
5References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 12, 1988
Grant dateJan 23, 1990
Priority date
Expiry dateMay 12, 2008

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L101/00
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Disclosed herein is a stretched poly(arylene thioether-ketone) film made of a thermoplastic material which comprises (A) 100 parts by weight of a melt-stable poly(arylene thioether-ketone) having predominant recurring units of the formula ##STR1## and having a melting point, Tm of 310.degree.-380.degree. C., a residual melt crystallization enthalpy, .DELTA.Hmc (420.degree. C./10 min) of at least 10 J/g and a melt crystallization temperature, Tmc (420.degree. C./10 min) of at least 210.degree. C., and a reduced viscosity of 0.3-2 dl/g as determined by viscosity measurement at 25.degree. C. and a polymer concentration of 0.5 g/dl in 98 percent by weight sufuric acid; and optionally, (B) up to 100 parts by weight of at least one of thermoplastic resins and/or up to 15 parts by weight of at least one of fillers. Its production process is also disclosed.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.