Novel spinning method
US4902492A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Oct 17, 1988 |
| Grant date | Feb 20, 1990 |
| Priority date | — |
| Expiry date | Oct 17, 2008 |
Classification
- Technology area (CPC D)Textiles; Paper
- CPC primaryD01F9/15
- WIPO fieldTextile and paper machines
- WIPO sectorMechanical engineering
Abstract
In a process for the production of carbon fibers from high boiling bituminous substances in which a purified and polymerized concentrated carbon fiber precursor is spun into fibers which are oxidized and then carbonized and optionally graphitized, the improvement comprising adding to the carbon fiber precursor just before spinning 2 to 10% by weight of a solvent in which the precursor is insoluble or only slightly soluble under normal conditions and mixing the resulting mixture under hypercritical conditions for the solvent for at least 10 minutes without gas or solid inclusions formed in the fiber and neoformatgion of solids is prevented.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.