Abstract
A gypsum mold having good water absorbing properties, which is suitable for cast molding pottery, can be prepared by stirring a mixture of hemihydrate gypsum cooled to -40.degree. to 5.degree. C. and water to form a slurry of gypsum in water having a temperature of -5.degree. to 10.degree. C., pouring it into a water-impermeable mold, maintaining it therein until the setting reaction thereof is completed and then releasing the set product from the mold.