Process for the chemical-thermal degradation of haolgenated hydrocarbons
US4937065A · kind A · utility
18Cited by
10References
8Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Dec 6, 1988 |
| Grant date | Jun 26, 1990 |
| Priority date | — |
| Expiry date | Dec 6, 2008 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S588/901
- WIPO fieldMachine tools
- WIPO sectorMechanical engineering
Abstract
Halogenated hydrocarbons are reacted in a reactor at temperatures up to 1000.degree. C. with greater-than-stoichiometric amounts of calcium and/or magnesium silicates in a reactor for the chemical-thermal degradation of the halogenated hydrocarbons. Neither dioxins nor furans are formed in the waste gas in this process.