Aluminum alloy and associated anode and battery
US4950560A · kind A · utility
Assignee
Inventor
Key dates
| Filing date | Aug 1, 1988 |
| Grant date | Aug 21, 1990 |
| Priority date | — |
| Expiry date | Aug 1, 2008 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/50
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
The present invention provides a eutectic aluminum base alloy and anode made therefrom which may include at least two elements from the group consisting of scandium, bismuth, cadmium, gallium, indium, lead, mercury, thallium, tin, and zinc. The alloying elements are present in the aluminum alloy in such quantity that they are at least in part liquid at the sites of local reaction on the anode. The preferred alloying components are eutectics of the elements. The alloys and anodes have a high overpotential for water reduction. The purity of the aluminum is preferably at least about 99.99%. Preferred compositions are aluminum-gallium-indium, aluminum-gallium-indium-tin, aluminum-gallium-indium-tin-zinc, aluminum-gallium-indium-zinc, aluminum-gallium-zinc, aluminum-gallium-tin, and aluminum-bismuth-cadium-indium-lead-tin. The alloying elements may preferably be present in a total amount of about 0.01 to 3.0 percent based on total alloy weight. In an alternate embodiment a molten anode may be employed.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.