Patent · US Expired

High temperature low friction seal

US4951954A · kind A · utility

28Cited by
6References
20Claims
0Family size

Assignee

Inventor

Key dates

Filing dateAug 23, 1989
Grant dateAug 28, 1990
Priority date
Expiry dateAug 23, 2009

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/215
  • WIPO fieldEnvironmental technology
  • WIPO sectorChemistry

Abstract

A high temperature low friction dynamic seal includes a wire mesh base portion and a compressed shell portion on the base portion. The shell portion includes between approximately 2% and 30% of high aspect ratio vermiculite having a mean particle size of less than approximately 50 microns, between approximately 10% and 88% of high temperature resistant fibers and between approximately 10% and 88% of one or more a solid lubricants selected from a group consisting of barium fluoride, calcium fluoride, cerium fluoride and a eutectic of barium fluoride and calcium fluoride. The method of forming the seal includes the steps of forming a compressed wire mesh base portion, applying an aqueous paste-like mixture of the shell portion components to the base portion, evaporating the water from the shell portion and compressing the shell portion and the base portion.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.