Articles utilizing acetal copolymer bonding resins

US4954400A · kind A · utility

6Cited by
3References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 11, 1988
Grant dateSep 4, 1990
Priority date
Expiry dateOct 11, 2008

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/31895
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

There are provided new articles comprising elements having surfaces bonded together with a bonding resin which is an elastomeric copolymer of about 15 to 45 mol %, preferably about 25 to 35 mol % trioxane, about 55 to 85 mol %, preferably about 65 to 75 mol % of 1,3-dioxolane, said mol percents based on the total of trioxane and 1,3-dioxolane, and about 0.005 to 0.15 wt. %, preferably about 0.05 to 0.12 wt. % of 1,4-butanediol diglycidyl ether or butadiene diepoxide as a bifunctional monomer, based on the total weight of copolymer. Preferably, at least one of said surfaces, and more preferably at least two of said surfaces bonded to each other are of a crystalline acetal polymer comprising at least 85 mol % of polymerized oxymethylene units.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.