Method of forming nickel foam

US4957543A · kind A · utility

37Cited by
12References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 16, 1989
Grant dateSep 18, 1990
Priority date
Expiry dateJun 16, 2009

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12486
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

The invention provides a nickel foam and a method of forming a nickel foam for a nickel containing battery. An open-cell foam structure is placed in a nickel carbonyl gas containing structure. The foam structure is heated to a temperature at which nickel carbonyl decomposes. Nickel from the nickel carbonyl gas decomposes on the foam structure to form a nickel plated foam structure. The nickel plated foam structure is then sintered leaving an open-cell nickel network to form the nickel foam. The open-cells of the nickel foam comprise substantially hollow wires having a substantially uniform transverse cross-section. The nickel foam is further characterized by the conductivity through the nickel foam multiplied by a factor of 3.4 being equal to or greater than the theoretical conductivity of nickel.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.