Patent · US Expired

Binder pitch and method of preparation

US4959139A · kind A · utility

13Cited by
17References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 9, 1989
Grant dateSep 25, 1990
Priority date
Expiry dateJan 9, 2009

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC10C3/00
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

Binder pitch is prepared by combining a petroleum aromatic mineral oil thermal tar and super finely subdivided calcined premium coke particles. The petroleum aromatic mineral oil thermal tar is obtained by hydrotreating, thermally cracking and vacuum distilling an aromatic mineral oil. Additionally, the aromatic mineral oil thermal tar may be subjected to heat soaking.