Superconducting wire and method of manufacturing the same
US4973574A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Apr 1, 1988 |
| Grant date | Nov 27, 1990 |
| Priority date | — |
| Expiry date | Apr 1, 2008 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T29/49014
Abstract
A method of manufacturing a superconducting wire is carried out by first preparing a material being composed of Y.sub.1 Ba.sub.2 Cu.sub.3 O.sub.7. This material is melted in a platinum crucible. A melt thus obtained is drawn out from a hole provided on the bottom wall of the crucible to be linearly discharged. The linearly discharged melt is cooled and solidified. A cooling/solidifying space for such a step is set at a temperature less by about 10.degree. C. than the solidifying point of the material, and a slow-cooling zone is provided next to the cooling/solidifying space. This slow-cooling zone is provided to be at a relatively high temperature in a portion closer to the hole while having a temperature gradient along a direction for linearly discharging the melt. A superconducting wire being composed of Y.sub.1 Ba.sub.2 Cu.sub.3 O.sub.7 is obtained. This superconducting wire superconducts at 85K.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.