Abstract

The present invention is in a sintered molding of partially stabilized zirconium oxide having a microstructure of 40 to 70 volume percent cubic phase, 30 to 70 volume percent tetragonal phase, and up to 10 volume percent monoclinic phase wherein the tetragonal phase is present in the form of precipitates less than 200 nm. A mixture of magnesia and yttria is used to stabilize the zirconia. Optionally, the sintered molding may further contain up to 20 wt. % spinel.