The invention provides a method of manufacturing a hydraulic hardening material having the steps of milling vitreous blast furnace slag and classifying the milled slag to provide slag powder having a blaine specific surface area of 6,000 to 12,000 cm.sup.2 /g. The hydraulic hardening material manufactured by the method is used as a Portland blast furance cement raw material.