Patent · US Expired

Process for shaping and improving the mechanical properties of blanks produced by powder metallurgy from an alloy with increased high-temperature strength by extrusion

US4992238A · kind A · utility

4Cited by
9References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 28, 1989
Grant dateFeb 12, 1991
Priority date
Expiry dateJul 28, 2009

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C21/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Process for shaping and improving the mechanical properties of blanks produced by powder metallurgy from an alloy with increased high-temperature strength by extrusion, and the deformation is successively performed in at least two temperature ranges different from one another or in two phases, in that the blank (2) is first reduced in its cross section at a temperature T.sub.1 and then is either agin reduced in at a lower temperature T.sub.2 or is deformed at a temperature T.sub.3 under counterpressure so that its cross section is further widened. T.sub.3 can be smaller than or equal to T.sub.1.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.