Abstract
A process for the production of a series 7000 aluminum alloy (Al-Zn-Cu-Mg) with a high level of mechanical strength and good ductility, by spray deposition. The object is the production of aluminum alloys having an ultimate stress.gtoreq.800 MPa and an elongation.gtoreq.5%, as well as the production of alloys which are reinforced by ceramic particles. According to the process, a solid alloy is formed by spray deposition, the alloy is transformed in the hot condition at between 300.degree. and 450.degree. C. and possibly in the cold condition, and the transformed alloy is subjected to solution treatment, quenching and aging.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.