Compositions for preventing stress cracks in poly(alkylene terephthalate) articles and methods of use therefor
US5009801A · kind A · utility
58Cited by
9References
14Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Aug 25, 1989 |
| Grant date | Apr 23, 1991 |
| Priority date | — |
| Expiry date | Aug 25, 2009 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC10N2050/01
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
Stress cracking in poly(alkylene terephthalate) articles of manufacture is prevented by applying to the article a hydrophilic-substituted aromatic hydrocarbon having either an alkyl or aryl side chain, such as, sodium xylene sulfonate. Preferably, the stress crack inhibitor is applied to the article in the form of an aqueous fatty acid-based lubricant.