Preparation of aqueous nonwoven binders of low formaldehyde emission on curing based on urea, formaldehyde and glyoxal
US5017641A · kind A · utility
3Cited by
6References
7Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | May 2, 1989 |
| Grant date | May 21, 1991 |
| Priority date | — |
| Expiry date | May 2, 2009 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G12/12
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Aqueous nonwoven binders that give reduced formaldehyde emission on curing are based on condensation products of urea or derivatives thereof, formaldehyde and glyoxal in a molar ratio, based on the solid binder, of from 1.5 to 2.5 moles of formaldehyde and from 0.1 to 0.5 mole of glyoxal per mole of the total urea used.