Method of filling a liquid crystal device with ferroelectric liquid crystal material
US5024255A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jul 21, 1988 |
| Grant date | Jun 18, 1991 |
| Priority date | — |
| Expiry date | Jul 21, 2008 |
Classification
- Technology area (CPC G)Physics
- CPC primaryG02F1/1341
- WIPO fieldOptics
- WIPO sectorInstruments
Abstract
An improved method of filling a liquid crystal device with a blended ferroelectric liquid crystal material is disclosed. The method includes the step of disposing the blended ferroelectric liquid crystal material in an inner space formed in the liquid crystal device, with the temperature of the blended liquid crystal being maintained during the disposing step at a temperature higher than the transition temperature of any constituent of the blended liquid crystal material such that the blended liquid crystal material is transformed in its isotropic phase.