Method for depositing highly erosive and abrasive wear resistant composite coating system on a substrate
US5024901A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | May 3, 1989 |
| Grant date | Jun 18, 1991 |
| Priority date | — |
| Expiry date | May 3, 2009 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/12944
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
The method for producing the disclosed material comprises chemical vapor depositing on the substrate a substantially columnar, intermediate layer of tungsten and chemical vapor depositing on the intermediate layer a non-columnar, substantially lamellar outer layer of a mixture of tungsten and tungsten carbide. The tungsten carbide comprises W.sub.2 C, W.sub.3 C, or a mixture of both wherein the ratio of the thickness of the tungsten intermediate layer to the thickness of the outer layer is at least: (a) 0.35 in the case of tungsten plus W.sub.2 C in the outer layer, (b) 0.6 in the case of a mixture of tungsten and W.sub.3 C in the outer layer and (c) 0.35 in the case of mixtures of tungsten and W.sub.2 C and W.sub.3 C in the outer layer. The chemical vapor deposition steps are carried out at pressures within the range of 1 Torr to 1,000 Torr and temperatures within the range of about 300.degree. to about 650.degree. C.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.