Abstract

An aluminum nitride sintered body mainly composed of aluminum nitride, contains 0.01 to 1.0 percent by weight of a rare earth element and 0.001 to 0.5 percent by weight of oxygen. Such a body has a thermal conductivity of at least 180 W/mK. For manufacturing such an aluminum nitride sintered body, aluminum nitride powder (201) is first prepared. At least one compound (203) containing a rare earth element is added to the aluminum nitride powder (201) to contain 0.01 to 1.0 percent by weight, in rare earth element conversion, of the compound. The ingredients are homogeneously mixed with each other. A green body is formed of the mixed powder and sintered at a temperature of 1500.degree. to 2200.degree. C. in a non-oxidizing atmosphere containing nitrogen.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.